Aluminum Suppliers & Grades

Wrought and cast aluminum alloys from 1100, 3003, and 5052 sheet to 6061, 2024, 7050, 7075, and MIC-6 cast tooling plate.

Aluminum is carried by almost every general line service center in the US, yet two quotes for '6061 bar' or 'aluminum tooling plate' can differ by 30~50% depending on whether the supplier quotes extruded T6511, cold-finished T651, domestic aerospace AMS plate, or cast MIC-6 jig plate.

Aluminum Grades & Trade Names

1000 Series

Live prices

Generic designation covering the 1xxx series (99%+ pure aluminum). Includes 1100, 1050, 1060, and similar commercially pure alloys. Extremely soft, excellent corrosion resistance, high thermal and electrical conductivity. Terrible machinability - gummy, stringy, and sticks to tooling. Used for chemical equipment, heat exchangers, and decorative applications. See 1100 for specific details.

1100

Live prices

Nearly pure aluminum (99%+). Extremely soft, gummy, and a nightmare to machine. Machinists compare it to cutting bubble gum. Produces terrible burrs, strings instead of chips, and welds itself to tooling. If you have to machine it, use razor-sharp HSS tools with high positive rake, flood coolant, and crank the SFM as high as you can. Mostly used for chemical equipment, food processing, and deep-drawn parts where corrosion resistance and formability matter more than machinability. If someone specs this for a machined part, ask if they actually need it or if 6061 would work. It almost always would.

1235

Live prices

Ultra-pure aluminum (99.35% minimum) used almost exclusively for foil and very thin gauge sheet. Not a machining alloy. If you encounter it, it's likely in thin sheet form for packaging, insulation, or capacitor applications. Compare to 1100 (similar purity, more common in thicker forms).

2011

Live prices

The free-machining aluminum. Lead and bismuth additions make this the closest thing aluminum has to 12L14 steel - chips break clean, surface finish is excellent, and tools last. Rated at around 90% machinability, tied with 6262 for the top spot among aluminum alloys. The tradeoff is corrosion resistance (worse than 6061) and it's essentially non-weldable. Used for high-volume screw machine parts: fittings, connectors, precision bushings, and anything that comes off an automatic lathe. If you're making 10,000 aluminum parts on a Swiss machine, spec 2011. Compare to 6262 (similar machinability, better corrosion resistance) and 6061 (standard shop alloy, much gummier to machine).

2014

Sourcing guide

High-strength aluminum-copper alloy (60+ KSI yield in T6) used heavily in aerospace structural forgings, heavy truck frames, and aircraft fittings. Machines cleanly with short chips similar to 2024 and 7075, and responds slightly better to resistance spot welding than 2024, though fusion welding is still discouraged and corrosion resistance requires Alclad or anodize protection.

2017

Sourcing guide

The original 'Duralumin' aluminum-copper alloy. Moderate-to-high strength with good machinability and chip breaking in T4/T451 bar, commonly specified for aircraft rivets, screw-machine fasteners, and legacy aerospace prints. Poor bare corrosion resistance and not suitable for fusion welding. Compare to 2024 (higher strength) and 2011 (faster screw-machining).

2024

Live prices

High-strength aluminum with copper as the primary alloying element. Machines well with good chip formation, closer to 7075 than 6061 in how it cuts. Excellent fatigue resistance, which is why it shows up constantly in aerospace structural parts like fuselage and wing components. The tradeoff is poor corrosion resistance (much worse than 6061) and it's essentially non-weldable. Typically needs protective coatings like Alclad in corrosive environments. Costs more than 6061, less than 7075, and sits between them in strength. If you need more strength than 6061 but your budget or application doesn't justify 7075, 2024 is worth considering.

2219

Sourcing guide

Weldable aluminum-copper aerospace alloy rated for both cryogenic liquid-fuel tanks and elevated temperatures up to 500°F. Unlike 2024, 2219 TIG-welds reliably with 2319 filler and responds well to post-weld heat treatment. Machines cleanly in T851/T87 tempers. Standard on launch vehicles, cryogenic plumbing, and supersonic structural skins.

3003

Live prices

Essentially pure aluminum with a bit of manganese. Designed for forming and drawing, not machining. In the shop, this stuff is soft, gummy, and smears on your tools. Machinists describe it as slightly better than 1100 but still miserable. It's the standard for deep drawing operations, beverage cans, and heat exchangers. If a customer specs 3003 for a machined part, it's usually because they need it for a subsequent brazing process. Hardened condition (H14, H18) machines a bit better than annealed, but don't expect clean cuts. Sharp tools, flood coolant, light cuts, and patience.

3004

Sourcing guide

Aluminum-manganese-magnesium sheet alloy with roughly 20% higher strength than 3003 while keeping good deep-drawing and roll-forming behavior. Primarily coil, sheet, and light plate for storage tanks, beverage can bodies, and architectural panels rather than CNC bar work.

3105

Live prices

A low-strength aluminum-manganese-magnesium alloy, primarily a sheet metal product. Better corrosion resistance than 3003 with slightly higher strength. Not a machining alloy. Shows up in building products like gutters, downspouts, siding, and roofing. If it ends up in your shop, it's being formed on a brake or run through a roll former, not turned on a lathe. Compare to 3003 (similar applications, slightly lower strength) and 5052 (significantly stronger, used when forming requirements are more demanding).

5000

Live prices

Generic designation covering the 5xxx series (aluminum-magnesium alloys). Non-heat-treatable alloys with good corrosion resistance, especially in marine environments. Strength depends on the specific grade: 5052, 5083, and 5086 are the most common. All are weldable and gummier to machine than 6061. See specific 5xxx grades for details.

5005

Live prices

Low-strength aluminum-magnesium alloy, mainly used for sheet metal and architectural applications. Similar to 3003 in machinability, meaning not great. Its main selling point is excellent corrosion resistance and a very clean anodized appearance, making it popular for anodized architectural trim and decorative panels. Not a machining alloy. If you see it in a shop, it's usually being formed or fabricated, not turned or milled. Think of it as 3003's slightly prettier cousin.

5052

Live prices

The workhorse of the marine aluminum world. Strongest of the common non-heat-treatable alloys, with excellent saltwater corrosion resistance. Better to machine in the hardened condition than annealed. Used heavily in boat hulls, decks, fuel tanks, and any application exposed to marine or chemical environments. Machines better than 3003 or 1100 but doesn't compare to 6061. Good weldability. If a job calls for aluminum in a corrosive environment and you can't heat treat, 5052 is likely the right call. Often compared to 5086 (which is stronger) and 6061 (which machines better but has less corrosion resistance).

5083

Live prices

The strongest non-heat-treatable aluminum. Excellent corrosion resistance, especially in seawater. This is the hull plate alloy for high-performance marine vessels and the standard for cryogenic tanks and pressure vessels. Machines better than you'd expect for a 5xxx alloy - the higher magnesium content (4.0 – 4.9%) gives it more body than 5052, so chips break a bit cleaner. Still gummier than 6061. Welds well with 5356 filler. About 10 – 15% stronger than 5086. If you're building anything that needs to survive saltwater and structural loading simultaneously, 5083 is likely on the drawing. Compare to 5086 (slightly weaker, otherwise similar) and 6061 (heat-treatable, better machinability, less marine corrosion resistance).

5086

Live prices

Stronger than 5052 with similar corrosion resistance, used in marine hulls and superstructures where more structural strength is needed. Not heat-treatable, so strength comes from work hardening. Welds well and retains most of its strength at the weld joint, which is a big deal in shipbuilding. Machinability is fair at best. Like most 5xxx alloys, it's softer and gummier than the heat-treatable 6xxx series. If 5052 isn't strong enough and you can't use 6061 because of corrosion concerns, 5086 fills the gap.

5454

Live prices

Similar to 5052 and 5086 but specifically rated for elevated temperature service (above 150°F), which is where 5083 and 5086 can become susceptible to stress corrosion cracking. This makes it the go-to alloy for pressure vessels, chemical tanks, and hot marine applications. Moderate strength, good weldability, decent corrosion resistance. Not a machining alloy. If you're building something that sees both heat and corrosive environments, 5454 is likely spec'd for a reason.

5456

Sourcing guide

High-magnesium marine structural aluminum (~5.1% Mg) offering slightly higher strength than 5083 in H116/H321 marine plate tempers. Weldable with excellent seawater resistance for ship hulls, armor plate, and offshore structures, though continuous service above 150°F is avoided due to sensitization.

6005

Live prices

An extrusion alloy that sits between 6063 and 6061 in strength. Developed specifically for thin-walled, complex extrusion profiles that need more structural performance than 6063 can deliver. Shows up in transit railcar frames, truck trailer structures, and architectural systems where the cross-section does the work. Machines adequately but like most extrusion alloys, it's designed to flow through a die, not sit in a chuck. If you're machining 6005, it's almost always secondary operations on an extruded profile. Compare to 6063 (weaker, better surface finish) and 6061 (stronger, the standard for bar stock).

6013

Live prices

Copper-modified 6xxx aerospace and defense alloy that delivers ~25% higher tensile strength than 6061-T6 while retaining good corrosion resistance, formability, and short-chip CNC machinability. Frequently specified for fuselage skins, hydraulic manifolds, and precision ordnance components.

6020

Sourcing guide

Lead-free free-machining 6xxx aluminum alloy alloyed with tin as a RoHS-compliant replacement for leaded 2011 and 6262 screw-machine bar. Breaks chips cleanly on Swiss and multi-spindle lathes and anodizes well.

6061

Live prices

The default aluminum for machine shops. If nobody specified an alloy, it's probably 6061-T6. Good strength, good corrosion resistance, welds well, and anodizes nicely. The machinability reputation is "good" but experienced machinists know it can be inconsistent lot to lot. Some batches cut clean, others get gummy and produce stringy bird's-nest chips, especially on lathes. 7075 actually chips better, but costs roughly twice as much per pound. 6061 is the alloy you reach for unless you have a specific reason not to. Compare to 7075 (stronger, chips better, costs more) and 6063 (weaker, better surface finish, designed for extrusions).

6063

Live prices

Often called "architectural aluminum." The most popular extrusion alloy because it flows through dies easily and produces excellent surface finishes. Softer and weaker than 6061, and less machinable. Can get gummy under the cutter in softer tempers. Its strength is in appearance, not performance. Anodizes beautifully with clean, uniform color. Window frames, door frames, railings, trim, and decorative profiles are its sweet spot. If you're machining 6063, it's usually because the part started as an extrusion and needs secondary operations, not because someone chose it as bar stock for a machined part.

6101

Live prices

Basically 6063 with minor chemistry tweaks to maximize electrical conductivity (55 – 60% IACS). The bus bar alloy. Used almost exclusively for electrical conductor applications like bus bars, power distribution, and switchgear. Half the weight of copper with over half the conductivity, which makes the math work for many electrical installations. Machines reasonably well for what it is. If you see 6101 in the shop, someone is making electrical components. Not a structural or general machining alloy.

6262

Live prices

Free-machining aluminum with lead and bismuth additions. Chemically similar to 6061 but with chip-breaking additives that make it dramatically easier to machine. Rated alongside 2011 as the best-machining aluminum alloy. Unlike 2011, it retains the good corrosion resistance and anodizability of the 6xxx family. Used for high-volume screw machine parts, fittings, valve bodies, and anything where cycle time on automatic lathes matters. Availability is tighter than 6061 or 2011, and it costs more. If you can get it, it's the best of both worlds: 6061 corrosion properties with 2011 machining characteristics. Compare to 2011 (similar machinability, worse corrosion resistance) and 6061 (readily available, gummier to machine).

6351

Sourcing guide

Structural aluminum extrusion and pipe alloy sitting just above 6061 in strength, historically common in seamless high-pressure gas cylinders, structural tubing, and heavy extruded shapes. Machines and welds much like 6061-T6.

7050

Live prices

High-strength aerospace aluminum, designed to fix 7075's biggest weakness: stress corrosion cracking in thick sections. Where 7075 can be unreliable in heavy forgings and thick plate over 3 inches, 7050-T7451 provides excellent SCC resistance with only a slight reduction in strength. This is wing spar material, bulkhead material, and heavy aerospace forging stock. Machines well like all 7xxx alloys - clean chips, good surface finish. More expensive than 7075 and available primarily in thick plate and forgings rather than standard bar stock. Compare to 7075 (slightly stronger in thin sections, less reliable in thick) and 2024 (lower strength, better fatigue resistance).

7075

Live prices

The strongest common aluminum alloy. Roughly twice the tensile strength of 6061 and machines noticeably better. Produces short, clean chips where 6061 strings. Leaves a brighter, smoother surface finish. The downsides: it costs about 2x what 6061 costs, it's essentially non-weldable, and it can be unstable in large hogouts due to residual stress from heat treatment. Standard in aerospace, defense, and anywhere you need maximum strength from aluminum. If 6061 can do the job, use 6061. Reach for 7075 when you need the extra strength or better machinability and can justify the price.

CAST TOOLING

Live prices

Cast aluminum plate designed specifically for machining fixtures, jigs, molds, and tooling. The key property is dimensional stability, not strength. Because it's cast rather than rolled, it has virtually zero internal stress, so it stays flat when you machine it. Where 6061 plate can warp and move as you remove material, cast tooling plate holds its shape. Produces small, uniform chips and machines consistently. Comes ground flat on both sides to tight tolerances (±.005"). MIC-6 (7xxx series) and ATP-5 (5083 based) are the two big names. If you're building a fixture or jig where flatness and stability matter more than raw strength, this is what you want.

MIC-6

Live prices

Alcoa's (now Arconic) brand name for cast aluminum jig plate, made from a 7xxx-series alloy. The critical property is dimensional stability - virtually no residual stress means it stays flat when you machine it. Comes precision ground on both sides to ±.005" thickness tolerance, ready to go straight into the fixture. The standard for vacuum plates, checking fixtures, jigs, molds, and any tooling plate where flatness matters more than raw strength. Machines consistently with small, uniform chips. Compare to ATP-5 (5083-based cast plate, different manufacturer, similar performance) and 6061 plate (cheaper but will warp during heavy hogouts).

US Suppliers That List Aluminum

Showing 5 of 112 suppliers in our directory. Filter by grade, shape, and ship-to state in Supplier Search.

Filter by state (112 total)

How Shop Buyers Choose an Aluminum Alloy

Quick side-by-side reference for common forms, shop applications, and purchasing pitfalls before you send out quotes.

GradeTypical Forms & SizesBest Shop FitWhat to Watch Out For
6061Extruded & cold-finished bar, T651 plate, sheet, structural angle/channel/tubeDefault general CNC machining, welded frames, manifolds, and anodized bracketsRolled T651 plate can bow during heavy one-sided hogouts; extruded T6511 bar is cheaper than cold-finished T651
MIC-6 / Cast Tooling PlatePrecision surface-ground cast plate (1/4 – 4 in thick, ±0.005 in flatness)Vacuum chucks, inspection fixtures, base plates, and router tables needing dead flatnessLower tensile/thread pullout strength (~24 KSI) and non-structural; do not use for flight load brackets
7075 & 7050T651/T7351 plate, cold-finished & extruded bar; 7050-T7451 thick plateHigh-strength aerospace hogouts, defense receivers, molds, and high-load linksRoughly 2x the price of 6061, non-weldable, and over 3 in thick aerospace parts usually switch to 7050-T7451
2024 & 2011T351/T4 bar, bare & Alclad sheet/plate (2024); T3 screw-machine bar (2011)High-fatigue airframe fittings (2024) and high-speed Swiss screw-machine parts (2011)Poor bare corrosion resistance (anodize or Alclad required) and non-weldable
5052 & 5083H32 sheet & plate (5052); H116/H321 marine plate (5083)Brake-formed enclosures, fuel tanks, weldments (5052), and saltwater boat hulls (5083)Gummy on CNC mills compared to 6061; specify 5052-H32 whenever tight sheet-metal brake bends crack 6061-T6
6063Architectural square/rectangular tube, pipe, angle, and T-slot extrusionsSharp-corner architectural frames, handrails, heatsinks, and cosmetic anodizingSquare-corner 6063-T52 tube has ~35% lower yield strength than radius-corner 6061-T6 structural tube

What to Specify on an Aluminum RFQ

Include these details on line 1 of your quote request so distributors price the same spec and surface finish.

Extruded (ASTM B221 / T6511) vs Cold-Finished (ASTM B211 / T651) bar

Extruded 6061-T6511 bar is noticeably cheaper for general milling and chucker turning, while cold-finished 6061-T6/T651 holds tighter diameter roundness for collet and Swiss bar feeders. State which one your job needs.

Cast jig plate brand equivalencies

Prints calling out 'MIC-6' often allow equivalent precision-ground cast tooling plates such as ATP-5, Alca-5, K100-S, or Vista-6. Confirming brand equivalency opens quotes across competing regional plate houses.

Standard sheet/plate blank sizes and PVC film

Standard aluminum sheet runs 48 x 96 in and 48 x 144 in (plus 60 x 144 in on marine/plate grades), and bar runs 12 ft (extruded shapes often 16 ft, 20 ft, or 24 ft). Request one-side or two-side PVC laser film on cosmetic 5052 sheet.

Domestic/AMS plate vs general import plate

Import 6061-T651 plate can save money on commercial machine bases, but inconsistent residual stress can potato-chip thin-wall pockets. Aerospace AMS 4027 and domestic mill plate machine more predictably on thin hogouts.

Frequently Asked Questions: Buying Aluminum

Why did my 6061-T6 sheet crack on the press brake?
6061-T6 is precipitation-hardened and cracks easily on tight inside bend radii (1T – 2T). Sheet metal enclosures and formed brackets are normally specified in 5052-H32, which bends cleanly to 1T while welding and resisting corrosion.
What is the difference between 6061-T6511 and 6061-T651?
Both are solution heat-treated, stretched for stress relief, and artificially aged, but T6511 is extruded bar/rod straightened after stretching (ASTM B221), whereas T651 applies to rolled plate or cold-finished bar (ASTM B209 / B211).
Is cast tooling plate (MIC-6 / ATP-5) cheaper than rolled 6061-T651 plate?
Per pound at the distributor, cast tooling plate usually costs slightly more than commercial 6061-T651 plate, but because both faces arrive precision-ground flat to ±0.005 in and free of rolling stress, shops skip face-milling cleanup and re-straightening.