Titanium Suppliers & Grades
Commercially pure (Grades 1, 2, 3, 4) and alloy titanium (Grade 5 Ti-6Al-4V, Grade 9 Ti-3Al-2.5V, Grade 23 ELI) bar, plate, sheet, and tube for aerospace, medical, and chemical applications.
Titanium sits in a concentrated specialty tier of the US supply chain. General line structural yards seldom hold titanium on the floor; aerospace, medical, and chemical shops source bar, plate, sheet, and seamless tube from titanium master distributors and AS9100 specialty houses.
Titanium Grades & Trade Names
Grade 1
Sourcing guideCommercially pure titanium (CP-1, UNS R50250). Lowest oxygen and iron content of all titanium grades, making it the softest (35 KSI yield) and most cold-formable titanium available. Chosen for plate heat exchangers, deep-drawn chemical vessels, chlor-alkali anodes, and explosion-clad plate where maximum ductility and corrosion resistance matter more than strength. Gummy on the lathe; use razor-sharp positive-rake uncoated carbide and flood coolant.
Grade 2
Live pricesCommercially pure titanium (CP-2). The workhorse grade for chemical processing and marine applications. Good corrosion resistance, moderate strength (50 KSI yield), and excellent weldability. Machines better than alloy grades but still demands respect. Use sharp, uncoated carbide (TiN coating is pointless on titanium since it's already titanium). Low speeds (50-100 SFM), aggressive feed, flood coolant (water-based, never chlorinated). Chips are thin and hot. They can catch fire if they pile up. Maintain positive rake and never let the tool dwell. Used for heat exchangers, chemical piping, marine hardware, and medical implants. Compare to Grade 5 (much stronger but more expensive) and 316 stainless (cheaper, adequate for many corrosion applications).
Grade 3
Live pricesCommercially pure titanium with higher oxygen content than Grade 2, giving about 15% more strength (65 KSI yield vs 50 KSI). Same corrosion resistance and weldability as Grade 2. Used when CP titanium's strength isn't quite enough but you don't need the jump to Grade 5. Less commonly stocked than Grade 2. Machines similarly to Grade 2. Compare to Grade 2 (more common, slightly lower strength) and Grade 4 (even stronger CP titanium).
Grade 4
Live pricesThe strongest commercially pure titanium (80 KSI yield). Highest oxygen content of the CP grades, which is what provides the strength increase. Same excellent corrosion resistance. Used for marine hardware, chemical processing, and high-strength fasteners where alloy titanium's cost isn't justified. Machines slightly harder than Grade 2 due to the higher strength. Compare to Grade 2 (weaker, more common) and Grade 5 (alloy titanium, significantly stronger).
Grade 5 (Ti-6Al-4V)
Live pricesTi-6Al-4V. The most common titanium alloy (90% of all titanium alloy production). 6% aluminum and 4% vanadium give a yield strength of 120+ KSI, more than double CP titanium. This is the aerospace titanium: airframe structural parts, engine components, landing gear, and fasteners. Also dominates medical implants (hip joints, bone screws). Machines harder than CP grades. Low speeds (40-80 SFM for turning), sharp uncoated carbide, aggressive feeds, and high-pressure flood coolant. Never stop the feed with the tool engaged. The heat builds instantly and destroys the insert. The most important machining rule: maintain chipload. Compare to Grade 2 (much weaker, much cheaper, better formability) and Grade 23 (ELI version, better fracture toughness).
Grade 9 (Ti-3Al-2.5V)
Live pricesTi-3Al-2.5V ('half 6-4', UNS R56320). Medium-strength alpha-beta titanium alloy (~90 – 105 KSI yield) engineered specifically to combine cold-drawability into seamless tubing with nearly twice the strength of CP Grade 2. Standard for aircraft hydraulic lines, motorsport exhausts, golf shafts, and performance bicycle frames. Welds and cold-bends far easier than Grade 5.
Grade 23 (Ti-6Al-4V ELI)
Live pricesTi-6Al-4V ELI (Extra Low Interstitial). Same 6-4 composition as Grade 5 but with tighter controls on oxygen, nitrogen, carbon, and iron. The reduced interstitial elements improve fracture toughness, ductility, and stress corrosion resistance, particularly at cryogenic temperatures. This is the medical implant grade, FDA-approved for surgical implants because the cleaner chemistry reduces risk of adverse tissue reaction. Also used for cryogenic vessels and aerospace structural components where damage tolerance is critical. Slightly more expensive than standard Grade 5. Machines the same. Compare to Grade 5 (standard version, adequate for most aerospace) and CP Grade 4 (much cheaper, adequate for non-structural implants).
US Suppliers That List Titanium
Showing 5 of 14 suppliers in our directory. Filter by grade, shape, and ship-to state in Supplier Search.
How Shop Buyers Choose a Titanium Grade
Quick side-by-side reference for common forms, shop applications, and purchasing pitfalls before you send out quotes.
| Grade | Typical Forms & Sizes | Best Shop Fit | What to Watch Out For |
|---|---|---|---|
| Grade 1 (CP-1) | Sheet, coil, thin plate, welded/seamless heat-exchanger tube | Deep drawing, plate heat exchangers, chemical anodes, and explosion cladding | Lowest strength (35 KSI yield) and very gummy on turning; overkill if cold forming isn't needed |
| Grade 2 (CP-2) | Sheet, plate, round bar, pipe, fittings, and weld wire | Chemical piping, seawater hardware, anodizing racks, and desalination vessels | 50 KSI yield matches mild steel; do not substitute where aerospace prints expect 120+ KSI Grade 5 |
| Grade 4 (CP-4) | Round bar, medical wire, strip, and plate | Dental implants, surgical hardware, and chemical fasteners needing unalloyed purity | Tighter warehouse availability than Grade 2 or Grade 5; verify bar diameter early |
| Grade 5 (Ti-6Al-4V) | Round/flat/hex bar, AMS 4911 sheet & plate, rings, and forgings | Airframe brackets, turbine hardware, motorsport fasteners, and subsea housings | AMS 4928 aerospace bar carries stricter ultrasonic/melt rules and higher cost than ASTM B348 commercial bar |
| Grade 9 (Ti-3Al-2.5V) | Cold-worked seamless hydraulic tube, thin sheet, and weld wire | Aircraft hydraulic tubing, exhaust systems, and high-fatigue tubular frames | Limited availability in heavy solid bar or thick plate; primarily a tubular and sheet alloy |
| Grade 23 (Ti-6Al-4V ELI) | Centerless-ground Swiss bar, wire, and medical/cryogenic plate | Orthopedic bone screws, spinal cages (ASTM F136), and cryogenic vessels | Standard Grade 5 cannot substitute on ASTM F136 surgical implant or AMS 4930 ELI drawings |
What to Specify on a Titanium RFQ
Include these details on line 1 of your quote request so distributors price the same spec and surface finish.
Exact specification tier (ASTM commercial vs AMS aerospace vs ASTM F-series medical)
Ordering 'Grade 5 1.5 in round bar' without a spec invites wide price spreads. ASTM B348 works for industrial/marine parts, AMS 4928 or AMS 4965 is required for aerospace airframes, and ASTM F136 covers surgical implants.
DFARS 252.225-7009 specialty-metal melt origin
Defense subcontracts require titanium melted in the United States or a DFARS qualifying country. Non-DFARS import sponge/bar often trades 20~40% lower on commercial work, so state melt rules on line 1.
Ultrasonic testing (UT) and surface finish
Aerospace rotating or fracture-critical parts frequently call out AMS 2631 Class A1 or AA ultrasonic inspection. Specify centerless-ground bar (±0.0005 in) for Swiss lathes vs peeled/rough-turned bar for chuckers.
Waterjet blanking vs full plate
Because Grade 5 plate is expensive per pound and work-hardens under thermal cutting, titanium houses routinely abrasive-waterjet near-net blanks so you only buy the part envelope rather than a full mill plate.
Frequently Asked Questions: Buying Titanium
- What is the price and spec difference between ASTM B348 and AMS 4928 Grade 5 titanium?
- Both cover Ti-6Al-4V bar, but AMS 4928 enforces aerospace melt practice, tighter microstructure and mechanical testing, and typically AS9100 lot traceability. If a commercial, racing, or marine print only calls out ASTM B348 Grade 5 without DFARS, letting suppliers quote commercial-spec bar avoids paying aerospace premiums.
- Can Grade 23 ELI substitute for standard Grade 5?
- Chemically, Grade 23 (Extra Low Interstitial) has lower maximum oxygen and iron than standard Grade 5, which improves fracture toughness but slightly lowers minimum tensile and yield minimums (120 KSI tensile vs 130 KSI on standard Grade 5). Never substitute either direction without written engineering approval on the spec.
- How are titanium bar and plate lengths typically sold?
- Titanium round bar is commonly supplied in 10 – 12 ft random lengths (or 6 – 12 ft precision Swiss ground bars), and most titanium service centers will saw-cut single blanks to length because per-pound value is high.