Nickel Alloys Suppliers & Grades
High-temperature and corrosion-resistant superalloys including Inconel 600, 625, and 718, Monel 400 and K-500, Incoloy 800H/825, and Hastelloy C-276 and C-22.
Nickel superalloys carry volatile nickel, molybdenum, cobalt, and niobium melt costs and long mill lead times. Most machine shops buy cut bar, forged rings, and waterjet plate blanks from superalloy master distributors rather than ordering full random lengths from general line warehouses.
Nickel Alloys Grades & Trade Names
A286
Live pricesAn iron-based superalloy (25.5% nickel, 15% chromium, 1.3% molybdenum, 2.15% titanium). Precipitation-hardenable to high strength while maintaining oxidation resistance to 1300°F. This is the budget superalloy. Much cheaper than nickel-based alternatives while providing adequate high-temperature performance. Used for jet engine cases, turbine wheels, fasteners, and springs at elevated temperatures. Machines moderately well in the annealed condition. Compare to Inconel 718 (higher temperature capability, more expensive) and 17-4 PH stainless (less temperature resistant but easier to source).
Alloy X
Live pricesHastelloy X (47% nickel, 22% chromium, 18.5% iron, 9% molybdenum). A high-temperature alloy with excellent oxidation resistance and strength up to 2200°F. Used for gas turbine combustion cans, afterburner components, furnace hardware, and petrochemical flash drums. Machines poorly like most nickel superalloys. Compare to Inconel 625 (better corrosion resistance, similar temperature range) and Inconel 600 (lower alloy content, less expensive, slightly lower temperature capability).
Hastelloy C-22
Live pricesHastelloy C-22 (56% nickel, 22% chromium, 13% molybdenum, 3% tungsten). Outstanding resistance to a wide range of aggressive chemicals including oxidizing and reducing acids, chloride-bearing solutions, and mixed-acid environments. Resists the widest range of chemicals of any nickel alloy. Machines very poorly, similar to Inconel 625. Used for chemical processing, pollution control, waste treatment, and pharmaceutical equipment. Compare to C276 (similar corrosion resistance, slightly different chemistry) and 625 (narrower chemical resistance but also used at higher temperatures).
Hastelloy C-276
Live pricesHastelloy C-276 (57% nickel, 16% chromium, 16% molybdenum, 4% tungsten). The original "will resist almost anything" superalloy. Exceptional resistance to pitting, stress corrosion cracking, and both oxidizing and reducing chemicals. Used for chemical processing, flue gas desulfurization, pulp and paper, and pharmaceutical manufacturing. Machines like other nickel superalloys, which is to say, badly. Sharp coated carbide, rigid setup, aggressive feed, flood coolant. One of the most expensive common engineering alloys. Compare to Alloy 22 (wider chemical resistance, newer formulation) and 625 (adequate for many of the same environments, slightly less expensive).
Hy Mu 80
Sourcing guideA high-permeability nickel-iron-molybdenum alloy (80% nickel, ~5% molybdenum). Designed for magnetic shielding applications where maximum permeability is required. Shields sensitive electronics, medical instruments, and scientific equipment from stray magnetic fields. Must be properly annealed after forming or machining to achieve optimal magnetic properties, because any cold work degrades permeability. Machine with care using sharp tools and light cuts to minimize residual stress. Not a structural or corrosion-resistant alloy. Compare to Mu Metal (similar 80% nickel composition, different brand name).
Incoloy 800H
Sourcing guideIncoloy 800H (32.5% nickel, 21% chromium, 46% iron). A high-temperature alloy with controlled carbon and grain size for superior creep and stress-rupture properties above 1100°F. Used for petrochemical furnace piping, heat exchangers, and reformer tubes. Machines like a tough austenitic stainless. Expect work-hardening and gummy chips, but less severe than Inconel grades because of the high iron content. Compare to Inconel 600 (better above 1800°F, more expensive) and 310 stainless (cheaper, adequate for less demanding high-temperature service).
Incoloy 825
Live pricesIncoloy 825 (42% nickel, 21.5% chromium, 30% iron, 3% molybdenum, 2.2% copper). Designed specifically for sulfuric and phosphoric acid service. The combination of nickel, chromium, molybdenum, and copper provides resistance to a broad range of corrosive environments. Less expensive than higher-nickel alloys like 625 or C276. Machines like a tough stainless, work-hardening but manageable with carbide. Used for chemical processing, pollution control, acid production, and oil and gas. Compare to 316 stainless (cheaper but inadequate in aggressive acids) and C276 (better overall corrosion resistance but much more expensive).
Inconel 600
Live pricesInconel 600 (76% nickel, 15.5% chromium, 8% iron). A high-temperature, corrosion-resistant nickel alloy that maintains strength and oxidation resistance up to 2000°F. This is furnace fixture material, heat treatment retort material, and nuclear steam generator tubing. Machines poorly. Think of the worst 304 stainless experience and multiply it. Extreme work-hardening, gummy chips, and rapid tool wear. Use sharp ceramic or coated carbide inserts, very rigid setups, high feeds, moderate speeds, and flood coolant. Compare to 304 stainless (much cheaper, adequate below 1500°F) and Inconel 625 (better corrosion resistance, even harder to machine).
Inconel 625
Live pricesInconel 625 (61% nickel, 21.5% chromium, 9% molybdenum, 3.6% niobium). The premium corrosion-resistant superalloy. Outstanding resistance to pitting, crevice corrosion, and stress corrosion cracking in aggressive environments. Maintains strength to 1800°F. Machines terribly, among the worst materials a shop will encounter. Ceramic inserts at low speed or sharp, coated carbide at very low SFM with aggressive feeds. Rigid machine, rigid setup, flood coolant. Tool life is measured in minutes, not hours. Used for chemical processing, marine exhaust systems, and nuclear applications. Extremely expensive. Compare to 316 stainless (adequate for mild environments, 10x easier to machine) and C276 (even better corrosion resistance).
Inconel 718
Live pricesInconel 718 (52.5% nickel, 19% chromium, 18.5% iron, 5% niobium, 3% molybdenum). The most widely used nickel superalloy. Precipitation-hardenable to very high strength (180+ KSI) while maintaining corrosion resistance and performance to 1300°F. This is jet engine turbine disk material, gas turbine material, and rocket engine material. Machines better than 625 or 600 in the solution-annealed condition, but still difficult. After aging it's extremely tough on tools. Ceramic inserts are common in production. Used extensively in aerospace, power generation, and oil and gas. Compare to Inconel 625 (not hardenable, better corrosion resistance, worse machinability) and Waspaloy (higher temperature capability).
Monel 400
Live pricesMonel 400 (67% nickel, 30% copper). One of the few alloys resistant to both hydrofluoric acid and seawater. Tough, corrosion-resistant, and difficult to machine. Work-hardens aggressively. Produces long, stringy chips that wrap around everything. Use sharp coated carbide, rigid setups, aggressive feeds, and flood coolant at 10%+ concentration. Don't let the tool dwell or rub. Used for marine hardware, chemical processing, oil and gas components, and anywhere you need to handle both acids and seawater. Expensive. Compare to 316 stainless (much cheaper, adequate for mild marine environments) and Inconel 625 (better at high temperatures).
Monel K-500
Live pricesMonel K-500. Precipitation-hardenable version of Alloy 400 that can be age-hardened to roughly HRC 30-35. Same excellent corrosion resistance as 400 but with significantly higher strength and hardness. Used for pump shafts, oil well tools, doctor blades, and marine fasteners where Monel 400 isn't strong enough. Harder to machine than 400 in the aged condition. Machine before aging when possible. Compare to Alloy 400 (softer, easier to machine) and 17-4 PH stainless (similar hardening concept but different corrosion profile).
Monel R-405
Live pricesMonel R-405. A free-machining version of Alloy 400 with controlled sulfur additions. Same nickel-copper composition and corrosion resistance as 400 but dramatically easier to machine. Chips break cleaner and tool life improves significantly. The sulfur does slightly reduce corrosion resistance in some environments. Used for high-volume machined parts requiring Monel properties: valve stems, pump shafts, and fittings. Compare to Alloy 400 (better corrosion resistance, much harder to machine) and Alloy 200 (pure nickel, different corrosion profile).
Nickel 200
Live pricesCommercially pure nickel (99.6%). Excellent corrosion resistance in reducing environments, particularly caustic alkalis. Good electrical and thermal conductivity. Machines tougher than you'd expect from a pure metal. The nickel wants to work-harden and produce long, gummy chips. Use sharp carbide, moderate speeds, high feed rates, and flood coolant. Similar machining approach to 304 stainless but slightly better chip formation. Used for chemical processing equipment, food processing, and caustic handling. Compare to Alloy 400 (stronger, better for mixed acid environments) and C110 copper (better conductivity, much worse corrosion resistance).
Nickel 201
Live pricesLow-carbon version of Nickel 200 (0.02% C max vs 0.15%). Designed for applications above 600°F where standard Nickel 200 can suffer from graphitization (carbon precipitation at grain boundaries). Same corrosion resistance and machinability as 200. Used for caustic evaporators, reactor vessels, and any high-temperature nickel equipment. If the part stays below 600°F, regular 200 works fine. Compare to Nickel 200 (same but for lower temperatures) and Alloy 400 (stronger, different corrosion profile).
US Suppliers That List Nickel Alloys
Showing 5 of 18 suppliers in our directory. Filter by grade, shape, and ship-to state in Supplier Search.
How Shop Buyers Choose a Nickel Alloy
Quick side-by-side reference for common forms, shop applications, and purchasing pitfalls before you send out quotes.
| Grade | Typical Forms & Sizes | Best Shop Fit | What to Watch Out For |
|---|---|---|---|
| Monel 400 & K-500 | Cold-drawn/hot-finished round & hex bar, plate, sheet, pipe | Seawater pump shafts, valve trim, marine fasteners, and hydrofluoric acid service | Monel 400 cannot harden by heat treat; step up to age-hardenable K-500 (or free-cutting R-405) for high-load shafts |
| Inconel 600 | Plate, sheet, round bar, and seamless furnace tube | Heat-treat retorts, furnace muffles, baskets, and dry chlorine/caustic service to 2000°F | Pits faster than 625 in wet chloride/acid environments; primarily a high-temperature oxidation alloy |
| Inconel 625 | Round bar, plate, sheet, pipe, weld overlay wire, and forgings | Subsea connectors, marine exhausts, sour-gas risers, and hot chloride scrubbers | ASTM B446 Grade 1 (annealed) vs Grade 2 (solution-annealed) alters high-temp creep ratings and availability |
| Inconel 718 | Solution-annealed or aged round bar, AMS sheet/plate, forged rings | Jet engine disks/fasteners (AMS 5662/5663) and oilfield downhole tools (API 6ACRA) | Aerospace AMS 5662/5663 (180+ KSI) and oilfield NACE MR0175 / API 6A (120 – 150 KSI) require completely different heat treatments |
| Hastelloy C-276 & C-22 | Plate, sheet, bar, pipe, and chemical fittings | Wet chlorine, ferric chlorides, mixed oxidizing/reducing acids, and pharmaceutical reactors | Severe work-hardening on the mill and lathe; budget extra carbide/ceramic inserts and slower cycle times |
| Incoloy 825 & 800H | Pipe, tube, plate, and round bar | Sulfuric/phosphoric acid piping (825) and 1100 – 1800°F petrochemical furnace tubes (800H) | Plain Alloy 800 lacks the controlled carbon and coarse grain required on ASME code 800H/800HT prints |
What to Specify on a Nickel Superalloy RFQ
Include these details on line 1 of your quote request so distributors price the same spec and surface finish.
Aerospace AMS vs oilfield NACE/API vs ASME pressure-vessel condition
On Inconel 718 alone, AMS 5662 (solution-annealed), AMS 5663 (aged), and API 6ACRA / NACE MR0175 oilfield bar are melted and aged to incompatible hardnesses (HRC 40+ aerospace vs HRC 32 – 36 max sour-gas). State the exact spec and condition.
Melt practice (VIM-VAR vs VIM-ESR) and DFARS origin
Rotating turbine and defense prints normally require double-vacuum melt (VIM + VAR or ESR) and DFARS 252.225-7009 qualifying-country melt. Confirm both on the MTR before cutting.
Saw-cut or waterjet net blanks vs full bars
At $18 – $55+/lb, buying a 12-foot bar for a 14-inch job locks thousands of dollars in shelf drop. Superalloy distributors routinely sell exact saw-cut slugs and waterjet rings with heat numbers Vibro-etched on each piece.
Quote validity and alloy surcharge window
Nickel and molybdenum surcharges reset monthly at the mills. Check quote expiration dates (often 3~7 days on superalloys) before locking in a multi-month customer PO.
Frequently Asked Questions: Buying Nickel Alloys
- Should a shop buy Inconel 718 solution-annealed (AMS 5662) or pre-aged (AMS 5663)?
- Heavy hogouts and deep-drilled components cut roughly twice as fast in solution-annealed AMS 5662 (~HRC 22 – 28), followed by outside precipitation aging (which shrinks parts predictably by ~0.0006 in/in). Short-run shafts or fasteners with light stock removal are often turned directly from pre-aged AMS 5663 using ceramic and Whisker/CBN inserts to skip outside heat-treat lead time.
- Are 'Inconel 625', 'Alloy 625', and 'UNS N06625' the same metal?
- Yes. 'Inconel' is Special Metals Corporation's registered trademark, while 'Alloy 625' and 'UNS N06625' are the generic chemistry designations produced by multiple domestic and European mills (such as Haynes, Carpenter, VDM, and ATI). Unless a print restricts approved mill sources, dual UNS/ASTM/AMS certification governs acceptance.
- When does Incoloy 825 make more sense than Hastelloy C-276?
- Incoloy 825 contains ~42% nickel and 30% iron (versus 57% nickel and 16% molybdenum in C-276), so it costs substantially less while still handling hot sulfuric acid, phosphoric acid, and sour gas where 316L stainless fails.
Already have a supplier quote in hand? Check if the price is fair.