Cast Iron Suppliers & Grades
Continuous-cast gray iron (Class 30, Class 40) and ductile iron (65-45-12, 80-55-06, 100-70-03) bar, plate, and rectangular stock for hydraulic manifolds, machine tool ways, and tooling.
Machine shops rarely buy sand castings for 1 – 50 piece hydraulic manifolds, bushings, or machine-tool ways anymore. Continuous-cast iron bar and rectangular stock (led in North America by Dura-Bar and Versa-Bar) gives fine, zero-porosity microstructure in saw-cut rounds, tubes, and milled manifold blocks.
Cast Iron Grades & Trade Names
65-45-12 Ductile Iron
Sourcing guideFerritic ductile iron (ASTM A536 65-45-12). Nodular graphite gives steel-like tensile strength and impact resistance with clean machinability and pressure tightness for 5,000 PSI hydraulic manifolds, cylinder glands, and rotary joints.
80-55-06 Ductile Iron
Sourcing guidePearlitic-ferritic ductile iron (ASTM A536 80-55-06). Higher strength and wear resistance than 65-45-12 for gears, bushings, sheaves, and heavy-load rotary components.
100-70-03 Ductile Iron
Sourcing guidePearlitic ductile iron (ASTM A536 100-70-03). High tensile strength (100 KSI min) and uniform through-hardening response (induction or flame hardens cleanly to HRC 50 – 55) for high-load cams, sprockets, rams, and forming rolls.
Class 30 Gray Iron
Sourcing guideContinuous-cast gray iron (ASTM A48 Class 30). Slightly softer and faster-machining than Class 40 with high graphite damping for low-to-medium pressure manifolds, pump housings, pistons, and fixture plates.
Class 40 Gray Iron
Sourcing guideContinuous-cast gray cast iron (ASTM A48 Class 40, Dura-Bar G2). Free-graphite flake structure provides natural vibration damping, lubricity, and clean, short-chip machining without burrs for machine-tool ways, gears, and hydraulic manifolds.
US Suppliers That List Cast Iron
Showing 3 of 3 suppliers in our directory. Filter by grade, shape, and ship-to state in Supplier Search.
How Shop Buyers Choose a Cast Iron Bar Grade
Quick side-by-side reference for common forms, shop applications, and purchasing pitfalls before you send out quotes.
| Grade | Typical Forms & Sizes | Best Shop Fit | What to Watch Out For |
|---|---|---|---|
| Class 30 Gray Iron | Continuous-cast rounds and rectangles | Low-pressure valve bodies, vibration-damping subplates, and fast-turning sleeves | Lower tensile strength (30 KSI min); Class 40 is far more widely carried by US distributors |
| Class 40 Gray Iron | As-cast & cold-finished rounds, rectangles, squares, and tubes | Machine-tool ways, gibs, vacuum chucks, glass molds, and medium-pressure manifolds | Brittle under tensile shock (zero elongation); use 65-45-12 ductile iron above ~3,000 PSI cyclic pressure |
| 65-45-12 Ductile Iron | Rounds, tubes, and proof-machined manifold rectangles | 5,000 PSI hydraulic manifolds, cylinder glands, rotary joints, and air-motor rotors | Machines ~15~20% faster and weighs ~10% less than 1018/4140 steel, but chips are longer than gray iron |
| 80-55-06 Ductile Iron | As-cast and turned rounds, tubes, and wear flats | Sheaves, gears, bushings, tie-rod nuts, and machine-tool spindles | Pearlitic-ferritic matrix is harder (~187 – 255 BHN) than 65-45-12; adjust carbide speeds accordingly |
| 100-70-03 Ductile Iron | Rounds and heavy rectangular bar | Induction/flame-hardened cams, sprockets, rams, and high-load rollers (hardens to HRC 50 – 55) | Tougher on drills and taps in the as-supplied 240 – 300 BHN range; confirm heat-treat target early |
What to Specify on a Cast Iron Bar RFQ
Include these details on line 1 of your quote request so distributors price the same spec and surface finish.
Continuous-cast vs sand-cast allowability
ASTM A48 (gray) and ASTM A536 (ductile) cover sand castings, while continuous-cast bar is routinely certified to ASTM A536 / Dura-Bar or Versa-Bar specs and passes ultrasonic/pressure tests far more reliably because it has no sand inclusions or centerline shrink.
As-cast vs proof-machined / cold-finished oversize
Raw continuous-cast bar carries an outer chill skin with +0.060 – +0.188 in cleanup allowance depending on diameter. Ordering pre-turned/peeled rounds or rotary-ground manifold blocks saves messy skinning passes and keeps abrasive cast-iron dust out of CNC ways.
Hydraulic manifold grain orientation
Continuous-cast rectangles solidify axially. Specify your finished L x W x H manifold envelope so the distributor saws from a bar cross-section that leaves uniform wall allowance on cross-drilled high-pressure ports.
Freight weight and palletizing
Manifold blocks add weight quickly (~0.26 lb/in³). Bundling multiple cut blanks onto one regional flatbed or fluid-power distributor shipment cuts LTL minimum freight charges sharply.
Frequently Asked Questions: Buying Cast Iron
- Why do hydraulic manifold shops prefer continuous-cast 65-45-12 over 1018 steel or sand castings?
- Compared to sand castings, continuous-cast bar has zero internal sand pockets or pinholes that leak at 3,000 – 5,000 PSI after 40 hours of cross-drilling. Compared to 1018 steel, 65-45-12 breaks chips cleanly without stringy internal cross-hole burrs, drastically cutting deburring labor.
- Are Dura-Bar and Versa-Bar interchangeable on ASTM prints?
- Both are North American continuous-cast iron producers supplying Class 40 gray iron and 65-45-12 / 80-55-06 / 100-70-03 ductile iron. Unless an OEM print locks in a single proprietary producer code without 'or equivalent', asking distributors to quote either brand widens regional floor availability.
- What stock lengths do continuous-cast iron bars come in?
- Full mill bars are normally 6 ft or 12 ft long (shorter in large diameters over 10 inches due to bar weight), and nearly every cast-iron distributor sells precision saw-cut slugs and milled 6-sided blocks.
Already have a supplier quote in hand? Check if the price is fair.